Журналы →  Non-ferrous Metals →  2015 →  №2 →  Назад

MATERIAL SCIENCE
Название Optimization of composition and properties of heat-resistant complex-alloyed aluminum alloy castings
DOI 10.17580/nfm.2015.02.09
Автор Mansurov Yu. N., Belov N. A., Sannikov A. V., Buravlev I. Yu.
Информация об авторе

Far Eastern Federal University, Vladivostok, Russia:

Yu. N. Mansurov, Professor, Head of a Chair of Material Science and Material Technology, e-mail: yulbarsmans@gmail.com

 

National University of Science and Technology “MISiS”, Moscow, Russia:
N. A. Belov, Professor of a Chair Casting Process Technologies
A. V. Sannikov, Post-Graduate Student of a Chair of Casting Process Technology

 

Far Eastern Federal University1, Vladivostok, Russia ; Institute of Chemistry of Far Eastern Branch of Russian Academy of Sciences3, Vladivostok, Russia:
I. Yu. Buravlev, Assistant Professor of a Chair of Material Science and Material Technology1, Researcher3

Реферат

Heat-resistant aluminum alloys are the high demand for a knowledge-based economy, because the development of new technology, operating at high temperatures, requires new casting alloys with high characteristics of heat resistance and light weight. Aluminium alloys belong to such group, including the most heat-resistant Al – Cu – Mn alloys (AM5 alloys). However, alloys of this system have low casting properties, which complicates the obtaining of complex shape thin-walled castings. Furthermore, during the prolonged operation at the temperatures of 250 oC and higher, this system alloys soften. The third serious deficiency of AM5 alloys (this also applies to a common type of silumin AK7ch (АК7ч) / AK9ch (АК9ч)) is a heat treatment of castings, including quenching (usually T6 and T7), which greatly affects the weaking of mechanical properties. This complication in the behavior of alloys requires the new solutions, such as a search for new original compositions based on eutectic doped with transition metals. As a result, the AN4Mts2 (АН4Мц2) alloy was developed on the basis of eutectics (Al) + Al3Ni. The analogue alloys of this type are called “nicalins”. The results of comparison of AN4Mts2 nicalin characteristics with the most heat-resistant industrial analogues (alloys on the basis of Al – Cu system and piston silumines) showed its higher long-term strength properties at the temperatures of 300–350 oC. Because of the high quality requirements of the charge and the high content of nickel, AN4Mts2 alloy can be considered as a model composition because its production requires high purity aluminum. Later a new heat-resistant nicalin AN2ZhMts (АН2ЖМц) was developed on the basis of Al – Ni – Fe – Mn – Zr system, where iron is the alloying component. Nevertheless, there are some unsolved problems: the optimal concentration of alloying elements is not defined in the developed alloy (including iron and impurities); conditions of obtaining of shaped castings with increased silicon content are not investigated; heat treatment regimes are not optimized. The information presented in this paper work is aimed at these problems' solving.

This work was carried out on the basic agreement and in a creative collaboration between the engineering center of National University of Science and Techcology “MISIS” and the Research and Education Center “NANO” Far Eastern Federal University.

Ключевые слова Aluminum, iron, impurities, aluminum alloys, heat resistance, poly-component system, casting, process step
Библиографический список

1. Anasyida A. S., Daud A. R., Ghazali M. J. Dry sliding wear behaviour of Al–12Si–4Mg alloy with cerium addition. Materials and Design. 2010. No. 31. pp. 365.
2. Bhattamishra A. K. Microstructural studies on the effect of Si and Cr on the intergranular corrosion in Al–Mg–Si alloys. Materials Design. 1997. No. 18. pp. 25–28.
3. Belov N. A., Sannikov A. V., Mishurov S. S., Belov V. D. Vliyanie kremniya na kharakter kristallizatsii i goryachelomkost zharoprochnogo liteynogo alyuminievogo splava AN2ZhMts (Influence of silicon on the nature of crystallization and hot-shortness of heat-resistant casting aluminium alloy AN2ZhMts (АН2ЖМц)). Tsvetnye Metally = Non-ferrous metals. 2011. No. 7. pp. 68–71.
4. Birbilis N., Buchheit R. G. Electrochemical characteristic of intermetallic phases in Al alloys. Journal of Electrochemical Society. 2004. Vol. 152. pp. 140–151.
5. Cevik E., Sun Y., Ahlatci H. Effect of peak-aged heat treatment on corrosion behavior of the AA6063 alloy containing Al3Ti. Archives of metallurgy and materials. 2012. Vol. 57, Iss. 2. pp. 469–477.
6. Mansurov Yu. N., Mamatkulov D. D., Kadyrova D. S., Aripova B. Kh., Buravleva A. A., Pimenov V. A. Struktura i svoystva tsvetnykh metallov i splavov (Structure and properties of non-ferrous metals and alloys). Tashkent : Publishing House of Academy of Sciences of Republic of Uzbekistan, 2014. 334 p.
7. Dudzik K. Mechanical properties of 5083, 5059 and 7020 aluminium alloys and their joints welded by MIG. Journal of KONES Powertrain and Transport. 2011. Vol. 18, No. 3. pp. 73–77.
8. Czechowski M. Effect of anodic polarization on stress corrosion cracking of some aluminium alloys. Advances in Materials Science. 2007. Vol. 7, No. 1(11). pp. 13–20.
9. Rana R. S., Purohit R., Das S. Reviews on the Influences of Alloying elements on the Microstructure and Mechanical Properties of Aluminum Alloys and Aluminum Alloy Composites. International Journal of Scientific and Research Publications. June 2012. Vol. 2, iss. 6. pp. 2250–3153.
10. Mostafapoor S., Emamy M., Malekan M. Effect of Ti–B Grain Refiner on Microstructure and Mechanical Properties of a New Super High Strength Aluminum Al–Cu–Mg–Zn Cast Alloy. Proceedings of 2015 International Conference on Chemical, Metallurgy and Environmental Engineering (CMAEE-15). Istanbul (Turkey), June 3–4, 2015. pp. 325–331.
11. Rana R., Purohit R., Das S. Reviews on the influences of alloying elements on the microstructure and mechanical properties of aluminum alloys and aluminum alloy composites. International Journals of Scientific Research Publications. 2012. Vol. 2(6). pp. 1–7.
12. Pourkia N. The effect of Ti and Zr elements and cooling rate on the microstructure and tensile properties of a new developed super highstrength aluminum alloy. Materials Science and Engineering: A. 2010. Vol. 527(20). pp. 5318–5325.
13. Jambukar G. B., Kharde Y. R. Study on Influences of Addition of Alloying Elements on Properties of Aluminium – Silicon Alloys: A Review. International Journal of Engineering Research and Applications. January-February 2013. Vol. 3, iss. 1. pp. 1808–1813.
14. Misra D. K., Tiwari R. S., Srivastava O. N. Devitrification of rapidly quenched Al–Cu–Ti amorphous alloys. Bulletin of Materials Science. August 2003. Vol. 26, No. 5. pp. 553–558.
15. Toleulova A. R., Smagulov D. U. Uprochnenie deformiruemykh splavov sistemy alyuminiy-tsirkoniy (Reinforcement of aluminium-zirconium system deformed alloys). Vestnik Kazakhskogo natsionalnogo tekhnicheskogo universiteta = Bulletin of Kazakh national technical university. 2011. No. 3 (85). pp. 192–197.
16. Wang P., Cui J., Lu G. Semi-solid Thixoforming Simulation of Al–Cu–Mn–Ti Alloy Parts via Any Casting. Journal of Material Science and Technologies. 2007. Vol. 23, No. 3. pp. 359–362.
17. Sannikov A. V., Belov N. A., Alabin A. N. Osobennosti kristallizatsii alyuminievogo splava AN2ZhMts (nikalina) pri lite v razlichnye formy (Peculiarities of crystallization of aluminium alloy AN2ZhMts (АН2ЖМц) (nikalin) during various mold casting). Liteyshchik Rossii = Russian foundry worker. 2013. No. 4. pp. 11–14.
18. GOST 30620–98. Splavy alyuminievye dlya proizvodstva porshney. Tekhnicheskie usloviya (State Standard 30620–98. Aluminium piston alloys. Specifications). Introduced: July 01, 2001. (in Russian)
19. GOST 1583–93. Splavy alyuminievye liteynye. Tekhnicheskie usloviya (State Standard 1583–93. Aluminium casting alloys. Spe cifications). Introduced: January 01, 1997. (in Russian)
20. Belov N. A., Belov V. D., Alabin A. N., Savchenko S. V., Novichkov S. B., Stroganov A. G., Tsydenov A. G. Liteynyy alyuminievyy splav — (ekonomnolegirovannyy vysokoprochnyy silumin) (Casting aluminium alloy — (lean alloyed high-strength silumins)). Patent RF, No. 2441091. Applied: March 01, 2013. Published: September 10, 2011. Bulletin No. 25.
21. GOST 9012–59. Metally. Metod izmereniya tverdosti po Brinellyu (State Standard 9012–59. Metals. Method of Brinell hardness measurement). Introduced: January 01, 1960. (in Russian)
22. GOST 1497–84. Metally. Metody ispytaniy na rastyazhenie (State Standard 1497–84. Metals. Methods of tension test). Introduced: January 01, 1986. (in Russian)