Journals →  Non-ferrous Мetals →  2016 →  #2 →  Back

MATERIAL SCIENCE
ArticleName Selection of an aluminum matrix composition for obtaining the heat treatable boron-aluminum alloys
DOI 10.17580/nfm.2016.12.07
ArticleAuthor Chervyakova K. Yu., Samoshina M. E., Belov N. A.
ArticleAuthorData

National University of Science and Technology “MISiS”, Moscow, Russia:

K. Yu. Chervyakova, Engineer of the “Casting Technologies and Materials” Engineering Center, Undergraduate of the Casting Process Technology Department
M. E. Samoshina, Senior Researcher of the “Casting Technologies and Materials” Engineering Center, Assistant Professor of the Casting Process Technology Department
N. A. Belov, Deputy Director of the “Casting Technologies and Materials” Engineering Center, Professor of the Casting Process Technology Department, e-mail: nikolay-belov@yandex.ru

Abstract

Problem of substantiating the aluminum matrix composition for obtaining the heat treatable boron-aluminum alloys in the form of ingots and sheet products. Aluminum-based materials alloyed by boron are promising radiation-resistant structural materials. Analysis of basic systems of the heat treatable (T6) aluminum alloys was carried out. Zinc-containing systems (Al – Zn – Mg and Al – Zn – Mg – Cu) has been excluded because of likelihood of burning-out at high smelting temperatures. With the use of the calculations (Thermo-Calc software) and experimental methods (including scanning electron microscopy and micropobe analysis), justified has been an unreasonableness of obtaining the boron-aluminum alloys based on magnesium-containing systems because of an active interaction of that element with boron. An (Al, Mg)B2 compound with particles of adverse needle-shaped form arises even at small magnesium concentrations. Experimental study has been focused on the boron-aluminum alloys based on Al – Zr – Sc (with magnesium, manganese and titanium additives) and Al – Cu systems. Alloys have been prepared on the base of high-purity aluminum in a graphite-fireclay crucible at the temperature of 900–950 оС in a RIELTEK («РЭЛТЕК») induction furnace, which provides an intensive melt mixing required to exclude a possibility of refractory boron-containing particles deposition. The melt was poured into a graphite moulds to obtain flat ingots of 40×120×200 mm in size. Samples for structural investigations has been cut thereof. Later on the ingots have been treated by strain and thermal processing. It was found that titanium introduction into the systems with zirconium and scandium doesn’t assist in preventing their interaction with boron, which hamper the aluminum matrix hardening. The Al – Cu system meets the requirements best of all since copper doesn’t interact with boron and doesn’t effect on composition of the boron-containing phases. It was determined that such system allows to obtain ingots and sheet products of aluminum boron-containing alloy possessing high mechanical properties. The maximum achievable hardness on ingots and sheet products amounts to 129 HV and 133 HV correspondingly, and the tensile strength (sheets) equals to 430 MPa.

This article was written within the implementation of the Agreement on subsidies No. 14.578.21.0004 (Unique identifierof the project RMEF157814X0004) between the National University of Science and Technology “MISiS” and the Ministry of Education and Science of the Russian Federation within the framework of realization of the Federal Target Program “Research and Development in the Priority Directions of Progress of the Scientific and Technological Complex of Russia for 2014–2020”, approved by the Decree of the Government of the Russian Federation of November 28, 2013, No. 1096.

keywords Boron-aluminum, sheet products, microstructure, thermal treatment, mechanical properties, hardness of alloy
References

1. Eichler J., Lesniak C. Boron nitride (BN) and BN composites for high-temperature applications. Journal of the European Ceramic Society. 2008, No. 28. рр. 1105–1109.
2. Peng Zhang, Yuli Li, Wenxian Wang, Zhanping Gao, Baodong Wang. The design, fabrication and properties of B4C/Al neutron absorbers. Journal of Nuclear Materials. 2013. No. 437. рр. 350–358.
3. Mohantya R. M., Balasubramaniana K., Seshadrib S. K. Boron carbide-reinforced alumnium 1100 matrix composites: Fabrication and properties. Materials Science and Engineering A. 2008. Vol. 498. рр. 42–52.
4. Lai J., Zhang Z., Chen X.-G. The thermal stability of mechanical properties of Al – B4C composites alloyed with Sc and Zr at elevated temperatures. Materials Science and Engineering A. 2012. Vol. 532. рр. 462–470.
5. Skibo Michael D., Schuster David M., Bruski Richard S. Apparatus for continuously preparing castable metal matrix composite material. Patent USA, No. 5531425. F27D27/00, B22D11/11, B01F7/16, C22C32/00, F27D3/00, C22C1/10, B22D1/00, C22C1/00. Patent holder : Alcan Aluminum Corporation. Asserted 07.02.1994. Published 02.07.1996.
6. Samoshina M. E., Belov N. A., Alabin A. N., Chervyakova K. Yu. Struktura i mekhanicheskiye svoystva listovogo prokata iz splava Al – 3% B, poluchennogo zhidkofaznym metodom (Structure and mechanical properties of alloy Al – 3% B flats, obtained by liquid-phase method). Tsvetnye metally = Non-Ferrous Metals. 2015. No. 10. pp. 19–24.
7. Ömer Sava, Ramazan Kayikci. Production and wear properties of metal matrix composites reinforced with boride particles. Materials & Design. 2013. Vol. 51 (October). pp. 641–647.
8. Belov N. A. Fazovyy sostav promyshlennykh i perspektivnykh alyuminievykh splavov (Phase composition of industrial and prospective aluminium alloys). Moscow : Publishing House of “MISiS”, 2010. 511 p.
9. Mondolfo L. F. Struktura i svoystva alyuminievykh splavov (Aluminium Alloys: Structure and Properties). Translated from English. Moscow : Metallurgiya, 1979. 640 p.

10. Kurbatkina E. I., Belov N. A., Alabin A. N., Sidun I. A. Osobennosti plavki i litiya bor-soderzhashchikh alumomatrichnykh kompositov na osnove splavov 6xxx serii (Peculiarities of melting and casting of boron-containing aluminum-matrix composites based on 6xxx alloys). Tsvetnye metally = Non-Ferrous Metals. 2015. No. 1. pp. 85–90.
11. Chen Xiao-Guang, Dube Ghyslain, Steward Nigel. Neutron absorption effectiveness for boron content aluminum materials. Patent US, No. 20080050270. G21F 1/08, C22B 21/00, C22C 21/00, C22C 32/00. Assertes 21.04.2005. Published 12.06.2007.
12. Alabin A. N., Belov N. A., Tabachkova N. Yu., Akopyan T. K. Heat resistant alloys of Al – Zr – Sc system for electrical applications: analysis and optimization of phase composition. Non-ferrous Мetals. 2015. No. 2. рр. 36–40.
13. Chen B. A., Pan L., Wang R. H., Liu G., Cheng P. M., Xiao L., Sun J. Effect of solution treatment on precipitation behaviors and age hardening response of Al–Cu alloys with Sc addition. Materials Science and Engineering A. 2011. Vol. 530. pp. 607–617.
14. Marquis E.A., Seidman D.N. Nanoscale structural evolution of Al3Sc precipitates in Al (Sc) alloys. Acta Materialia. 2001. Vol. 49. pp. 1909–1919.
15. Yasuhiro Aruga, Katsura Kajihara, Yasuaki Sugizaki. Aluminum base alloy containing boron and manufacturing method thereof. Patent US. No. 7125515. B22D 30/00, C22F 1/04. Asserted 15.04.2003. Published 24.10.2006.
16. Belov N. A., Samoshina M. E., Alabin A. N., Chervyakova K. Yu. Vliyanie medi i magniya na strukturu i fazovyi sostav slitkov boraluminiya (Copper and magnesium effect on structure and phase composition of boron-aluminum ingots). Metally = Metals. 2016. No. 1. pp. 86–92.
17. Belov N. A., Alabin A. N. Termostoykiy splav na osnove aluminiya i sposob polucheniya iz nego deformirovannykh polufabrikatov (Aluminum base heat-resistant alloy and strained half-finished product manufacturing method thereof). Patent RF, No. 2446222. IPC С22С 21/14, С22F 1/057. Patent holder : National University of Science and Technology “MISiS”. Asserted 29.10.2010. Published 27.03.2012.
18. Alabin A. N., Belov V. D., Belov N. A., Mishurov S. S. Termostoykiy liteynyi aluminievyi splav (Heat-resistant casting aluminum alloy). Patent RF, No. 2478131. IPC В82В 3/00, С22С 21/06. Patent holder : National University of Science and Technology “MISiS”. Asserted 29.10.2010. Published 27.03.2012.

Full content Selection of an aluminum matrix composition for obtaining the heat treatable boron-aluminum alloys