PHYSICAL CHARACTERISTICS AND THEIR STUDY
Название Changes of structural characteristics during heating of of Bi0,4Sb1,6Te3 solid solution
Автор K. V. Gochua
Информация об авторе K. V. Gochua, National University of Science and Technology «MISiS».
Реферат The aim of this study is to select a heating mode for which the growth of Bi0,4Sb1,6Te3 (p−type) grains would be insignificant, and the nanoscale size would be retained (particle size less than 100 nm) while obtaining mechanically tough bulk Bi0,4Sb1,6Te3 (p−type). I show that a complete dissolution of the excess tellurium occurs at 250 °C and above, and a spinodal decomposition takes place at temperatures of above 400 °C.
Ключевые слова Bismuth telluride, thermoelectric properties, structure, figure of merit, excess tellurium, spinodal decomposition, pressing method.
Библиографический список
1. Sootsman, J. R. Strong reduction of thermal conductivity in nanostructured PbTe prepared by matrix encapsulation / J. R. Sootsman, R. J. Pcionek, H. Kong, C. Uher, M. G. Kanatzidis // Chem. of Mater. - 2006. - V. 18, N 21. - P. 4993—4995.
2. Gol'tsman, B. M. Poluprovodnikovye termoelektricheskie materialy na osnove Bi2Te3 / B. M. Gol'tsman, V. A. Kudinov, I. A. Smirnov - M. : Nauka, 1972. - 320 s.
3. Holopkin, A. I. Theoretical estimation of characteristics of thermoelectric materials made of nanopowders / A. I. Holopkin, V. N. Abrutin, V. A. Romanko, P. V. Miroevskiy, I. A. Zotov // Proc. 5th Europ. Conf. on Thermoelectrics. 2007.
4. Gusev, A. I. Attestatsiya nanokristallicheskikh materialov po razmeru chastits (zeren) / A. I. Gusev, A. S. Kurlov // Metallofizika i noveyshie tekhnologii. - 2008. - T. 30, № 5. - S. 679—694.
5. Gorelik, S. S. Rekristallizatsiya metallov i splavov / S. S. Gorelik, S. V. Dobatkin, L. M. Kaputkina - M. : Metallurgiya, 1967. - 432 s.